Ghosting / Shadow After Press

low
press
peel

Double image from press movement or inadequate cooldown on cold peel.

Likely Causes

  1. Press movement on open: Sliding before bond sets.

  2. Cold-peel performed too early: Adhesive not set; film drags design.

  3. Uneven pressure/warped platen: Partial bond and creep.

  4. Garment rebound/stretch: Moves graphic during peel.

Quick Checks

  • Hold press stable; avoid sliding before cooldown.
  • Respect cold-peel wait time strictly.

Step-by-Step Fix

  1. Install non-slip silicone padPrevents lateral slide on open.

  2. Follow rated peel mode strictlyAllows adhesive to set fully.

  3. Adjust pressure to even, medium-firmEnsures uniform bond.

  4. Support garment during peelReduces rebound movement.

  5. Post-press 2–3 s with parchmentLocks surface finish and bond.

Acceptance Criteria
  • No shadow at 12 in / 30 cm.