Shaker Over-Applying Powder

medium
shaker
powder

Excess powder from high vibration/gate height → orange peel after cure.

Likely Causes

  1. Shaker vibration is set too high: Dispenses too much powder.

  2. Feed gate is open too wide: Allows an excessive amount of powder to fall.

Quick Checks

  • Lower vibration or gate; weigh powder per square foot.
  • Check feed auger timing.

Step-by-Step Fix

  1. Reduce feed rate and vibration 10–20%Targets spec spread

Acceptance Criteria
  • Smooth surface, no pebbling on rub test